What Is PTC Intensity (Rmax/R20)? The ≥10³ Rule Explained (2026)

  • This topic is empty.
Viewing 1 post (of 1 total)
  • Author
    Posts
  • #13645
    admin
    Keymaster

      When a datasheet says a film is self-limiting and stops there, the single most useful follow-up question is what is PTC intensity Rmax R20 ratio. PTC intensity is the peak resistance a film reaches divided by its resistance at 20 °C. A ratio of 1 means the material is essentially a fixed resistor; a ratio of 10³ means resistance climbs a thousandfold before it turns over, which is what actually chokes current and holds temperature. YOTTECH, the export brand of Jiangsu Yottuo New Materials Co., Ltd., publishes this metric because a buyer cannot verify self-regulation without it.

      The GB/T 29470 PTC strength 10 to the power of 3 requirement is a floor, not a target. It says a qualifying self-limiting electric heating sheet must reach at least 10³ between its cold resistance and its maximum resistance. Published carbon systems sit well above it: carbon-black/HDPE loaded with Ensaco 150G changes resistance by 10⁶ from room temperature to 130 °C, and HDPE filled with carbon fibre reaches the 10¹⁰ Ω·cm order in the peak region. A supplier who quotes only a switching temperature has not told you how steep the curve is.

      Published: November 16, 2026 | By YOTTECH Engineering Team

      Resistance-temperature curve showing the peak-to-cold ratio used for PTC strength

      1. What does Rmax/R20 measure, and why does the 10³ floor matter?

      It measures how far the material can throttle itself: R20 is the resistance at 20 °C, Rmax is the highest resistance before the curve bends back down, and their ratio is the PTC strength. Under constant voltage, power is V²/R. If resistance rises a thousandfold, steady power falls to roughly a thousandth of the cold inrush, so the film settles instead of running away. If the ratio is only 3 or 5, the film warms but never truly regulates — it just becomes a slightly losing resistor.

      ✅ R20 is measured at 20 °C after the lot has stabilised, not at the coldest shipping temperature.

      ✅ Rmax is the true peak on the R-T trace, which is not always at the quoted switching point.

      ✅ The ratio is measured on the production lot, because filler dispersion and crosslinking shift it batch to batch.

      ✅ Published academic values span 10³ to 10⁶; a three-order rise is the credible entry threshold, not a marketing extra.

      This is where the vocabulary gets slippery. The authoritative Curie-point definition from Murata describes the temperature at which resistance doubles from its 25 °C value — a definition written for ceramic thermistors, not flexible heater film. Beyond the peak, resistance turns downward again at the TN point. Above TN, a self-limiting film quietly becomes a positive-feedback heater. That is why any answer to what is PTC intensity Rmax R20 ratio should be accompanied by the full R-T trace and an explicit TN point, not a single number.

      Crosslinking decides whether the curve has a useful peak at all. Unirradiated carbon-black polyethylene tends to show NTC behaviour; electron-beam irradiation converts it to PTC and suppresses the negative slope on later cycles. One study of EB-irradiated ionomer/CB-HDPE reported an intensity ratio of 3.01, roughly 35% higher than the unirradiated control, while a three-component YWO/graphene/silicone system reached a 945.92% resistance change and held temperature within 3.65 ± 1.05 °C. None of these numbers transfer automatically to your film, but they show the range a real formulation house can engineer.

      ✅ Bottom line: Treat Rmax/R20 as the definition of self-limiting — below 10³ the film regulates poorly, and no peak means no regulation.

      2. How do you measure PTC strength on a production lot?

      Heat a coupon through the transition slowly, hold at each step until resistance stops drifting, and record the complete curve — a fast ramp will understate Rmax and flatter a weak formulation. The method published in T/CGIA 033-2020 runs 20 to 100 °C in 5 °C increments, ramps at 0.5-1 °C per minute, and holds 10 minutes at each plateau. That dwell is the part most shortcut reports omit, and it is the part that separates a real peak from thermal lag.

      How to measure PTC strength of heating film starts before the oven: condition the sample, measure R20 with a four-wire method if the sheet is low-resistance, then log resistance against a thermocouple bonded to the film itself rather than to the chamber air. Chamber temperature and film temperature diverge by several degrees during a transition, and using air temperature shifts the apparent switch point.

      ✅ Ask for the trace, not a summary — a single "PTC strength ≥10³" line hides where the peak sits and how sharply it falls.

      ✅ Confirm the ramp rate and dwell time; a 5 °C/min sweep is not comparable to a 0.5 °C/min one.

      ✅ Repeat on at least three coupons from different positions in the roll to catch coating gradients.

      ✅ Pair the curve with insulation and leakage data; a strong PTC peak cannot excuse weak dielectric performance.

      How to measure PTC strength of heating film also means agreeing whose standard you are quoting. GB/T 29470 is a Chinese national standard; the GB/T 29470 PTC strength 10 to the power of 3 requirement is useful evidence of a regulated material, but it is not global certification and should not be presented as CE, UL or IATF approval. For an OEM program, request the lot curve plus the dielectric and ageing reports, and ask your supplier to evidence any additional automotive approvals your customer requires.

      At YOTTECH, the R-T trace is treated as a lot document rather than a brochure figure. Our carbon-based PTC heating film range is built on conductive carbon black, graphite, graphene or CNT systems in PET or PI, and Jiangsu Yottuo New Materials Co., Ltd. holds CQC product certification for electric heating film. We supply OEM and ODM custom grades with lot-specific curves, a sample plan for validation and wholesale pricing from our 5,000 m² factory in Xinyi. Details of the certification scope are on our support page.

      ✅ Bottom line: Demand the full R-T trace with ramp rate, dwell and lot ID — the ratio is only as honest as the method behind it.

      Frequently Asked Questions

      Q: what is PTC intensity Rmax R20 ratio in plain terms?

      A: It is the peak resistance divided by the resistance at 20 °C. A ratio of 10³ means the film can cut its own power by about a thousand times as it warms; that is the mechanism behind self-limiting behaviour.

      Q: Is a higher PTC strength always better?

      A: Not automatically. A very steep transition can make warm-up slow and the switch point sensitive to substrate and mounting. Match the ratio and switching temperature to the application, then verify stability over cycles rather than chasing the largest number.

      Q: Can I get the R-T curve before placing a volume order?

      A: Yes. YOTTECH provides lot-specific R-T data with custom sample rolls, so you can confirm the ratio and TN point on your own coupon before mass production. Contact our engineering team with your voltage, target temperature and substrate.

      Request the Lot R-T Curve Before You Qualify a Film

      Send YOTTECH your target switching temperature, voltage and film thickness. We will return a measured R-T trace, the Rmax/R20 calculation, a sample plan and factory-direct pricing for OEM programs — within one working day. YOTTECH also supports custom filler systems and MOQ-friendly trial rolls.

      http://www.yotthermo.com
      Jiangsu Yottuo New Materials Co., Ltd.

    Viewing 1 post (of 1 total)